Abstract
Ishda qalinligi 1,3 mm bo‘lgan AlSi qoplamali HS1300T/950Y MS AS60G60G martensitli po‘latni Prima Power LASER NEXT 1530 fiber lazer stanogida kesishda shlak hosil bo‘lishi tadqiq etilgan. Taguchi L9(3⁴) va Box–Behnken rejalari asosida azot va kislorod muhitida tajribalar o‘tkazildi, ANOVA yordamida omillarning ta’sir ulushlari aniqlandi va shlak massasining ikkinchi tartibli regressiya modeli qurildi. Optimal rejimda (P = 1980 Vt, v = 8,8 m/min, p = 14,2 bar N₂, f = −0,6 mm) shlak massasi 72 % ga kamaydi va ISO 9013:2017 bo‘yicha 1-diapazon sifati ta’minlandi.
References
1. Karbasian H., Tekkaya A.E. A review on hot stamping // Journal of Materials Processing Technology. — 2010. — Vol. 210, № 15. — P. 2103–2118.
2. Bach J., Zeuner A.T., Wanski T. va b. Influence of dross on the fatigue strength of laser-cut AISI 304 // 2023.
3. Russo Spena P. CO₂ laser cutting of hot stamping boron steel sheets // Metals. — 2017. — Vol. 7, № 11. — 456.
4. Steen W.M., Mazumder J. Laser Material Processing. — 4th ed. — London: Springer, 2010. — 558 p.
5. Григорьянц А.Г., Шиганов И.Н., Мисюров А.И. Технологические процессы лазерной обработки. — М.: МГТУ им. Н.Э. Баумана, 2006. — 664 с.